Creep test
Creep Testing Facilities
Submitted by shiva on Thu, 08/19/2010 - 17:09
Area Linked to:
Materials Evaluation
Research Area:
Mechanical Behaviour of Materials NML has the largest creep testing facility in South-East Asia with a total of 193 creep testing points. Out of these 61 units are 3T single creep points with a maximum temperature capability of 950oC to 1100oC and 11 units are multi creep points in which 12 specimens can be tested simultaneously in each unit at a temperature of 900oC.
Year of Installation:
1974 